王胜利,岳智勇,王冲锋.全钢载重子午线轮胎外观缺陷的原因分析及改善措施[J].橡胶科技,2021,19(7):0347-0350. |
 二维码(扫一下试试看!) |
全钢载重子午线轮胎外观缺陷的原因分析及改善措施 |
Cause Analysis and Improvement Measures of Appearance Defect of Truck and Bus Radial Tire |
投稿时间:2021-03-02 修订日期:2021-03-02 |
DOI:10.12137/j.issn.2095-5448.2021.07.0347 |
中文关键词: 全钢载重子午线轮胎 外观缺陷 外观色差 胶边 胎侧缺胶 模具 改善措施 |
英文关键词: truck and bus radial tire appearance defect appearance color difference rubber rim rubber lack on sidewall mold improvement measure |
基金项目: |
中图分类号: |
|
摘要点击次数: 1496 |
全文下载次数: 6 |
中文摘要: |
研究全钢载重子午线轮胎外观缺陷的主要原因和改善措施。对外观色差、胶边大、胎侧缺胶等轮胎外观缺陷问题,从轮胎工业化设计、工艺参数和设备精度等方面进行原因分析,并提出相应的改善措施,提高了成品轮胎外观的一次合格率和外观品质,降低了成品轮胎的缺陷率。 |
英文摘要: |
The main causes and improvement measures of appearance defects of truck and bus radial tire were studied.For the appearance defects of tire such as color difference,large rubber rim and rubber lack on sidewall,the reasons were analyzed from the aspects of tire industrial design,process parameters and equipment precision,and the corresponding improvement measures were put forward,which improved the first pass rate and appearance quality of finished tire,and reduced the defect rate of finished tire. |
|