文章摘要
刘 辉,张明香.轮胎过热水硫化上下模温差的研究[J].橡胶科技,2024,22(7):0410-0413. 本文二维码信息
二维码(扫一下试试看!)
轮胎过热水硫化上下模温差的研究
Study on Temperature Difference Between Upper and Lower Mold of Tire Vulcanization with Superheated Water
投稿时间:2023-12-14  修订日期:2023-12-14
DOI:10.12137/j.issn.2095-5448.2024.07.0410
中文关键词: 轮胎  过热水  硫化  中心机构  压盖  喷孔角度  上下模温差
英文关键词: tire  superheated water  vulcanization  center mechanism  pressure cover  spray hole angle  temperature difference between upper and lower mold
基金项目:
中图分类号:
作者单位E-mail
刘 辉* 双钱集团(新疆)昆仑轮胎有限公司 564545066@qq.com 
张明香 双钱集团(新疆)昆仑轮胎有限公司  
摘要点击次数: 956
全文下载次数: 381
中文摘要:
      为解决轮胎过热水硫化工艺中温差大问题,对硫化机中心机构压盖喷孔角度进行改进,并进行轮胎硫化测温试验。结果表明,中心机构压盖喷孔垂直、水平倾角均为15°可在内压蒸汽阶段减少低温冷凝水的产生,从而降低轮胎上下模温差。
英文摘要:
      In order to solve the large temperature difference problem during the superheated water vucanization process of tire,the angle of the pressure cover spray hole of the vulcanization press center mechanism was improved,and tire vulcanization temperature measurement tests were conducted.The results showed that the vertical and horizontal inclination angles of the pressure cover spray holes of central mechanism were both 15°,which could reduce the generation of low-temperature condensed water during the internal pressure steam stage,and reduce the temperature difference between the upper and lower molds of the tire.
Author NameAffiliationE-mail
LIU Hui DOUBLE COIN GROUP(XIN JIANG)KUNLUN TYRE CO.,LTD. 564545066@qq.com 
ZHANG Mingxiang DOUBLE COIN GROUP(XIN JIANG)KUNLUN TYRE CO.,LTD.  
查看全文   查看/发表评论  下载PDF阅读器