张 鹏,张建新,张 超,张志坚.全钢载重子午线轮胎胎侧蛇形弯曲原因分析及解决措施[J].橡胶科技,2024,22(1):0045-0047. |
 二维码(扫一下试试看!) |
全钢载重子午线轮胎胎侧蛇形弯曲原因分析及解决措施 |
Causes and Solution Measures of Snake Bend on Sidewall of All-steel Truck and Bus Radial Tire |
投稿时间:2022-10-03 修订日期:2022-10-03 |
DOI:10.12137/j.issn.2095-5448.2024.01.0045 |
中文关键词: 全钢载重子午线轮胎 胎侧 蛇形弯曲 胎圈 |
英文关键词: all-steel truck and bus radial tire sidewall snake bend bead |
基金项目: |
中图分类号: |
|
摘要点击次数: 1718 |
全文下载次数: 621 |
中文摘要: |
对全钢载重子午线轮胎胎侧蛇形弯曲的产生原因进行分析,并提出相应解决措施。通过采取胎侧在恒温恒湿环境下停放、调整挤出机温度匹配性、合理设定混炼胶门尼粘度标准、优化耐磨胶配方及改进胎侧终口型系数等措施,有效解决了胎侧蛇形弯曲问题,降低了胎侧部件返工率,使成品轮胎胎圈类质量缺陷的理赔率由0.66%下降至0.21%。 |
英文摘要: |
The causes of snake bend on the sidewall of all-steel truck and bus radial tire were analyzed,and the corresponding measures were proposed.By adopting measures such as parking the sidewall in a constant temperature and humidity environment,adjusting the temperature matching of the extrusion mschine,reasonably setting the Mooney viscosity of the compound,optimizing the wear-resistant compound formula and improving the sidewall final die openning coefficient,the problem of snake bend on the sidewall had been effectively solved,the rework rate of sidewall components was reduced,and the claim rate for quality defects in finished tire beads decreased from 0.66% to 0.21%. |
|