张丽丽,花曙太,邢涛,陈雪梅.改性203树脂在半钢子午线轮胎胎侧胶中的应用[J].橡胶科技,2020,18(7):0386-0388. |
 二维码(扫一下试试看!) |
改性203树脂在半钢子午线轮胎胎侧胶中的应用 |
Application of Modified 203 Resin in Sidewall Compound of Steel-belted Radial Tire |
投稿时间:2020-04-15 修订日期:2020-04-15 |
DOI:10.12137/j.issn.2095-5448.2020.07.0386 |
中文关键词: 半钢子午线轮胎 胎侧胶 酚醛增粘树脂 粘性 生热 滚动阻力 |
英文关键词: steel-belted radial tire sidewall compound phenolic tackifier viscosity heat build-up rolling resistance |
基金项目: |
中图分类号: |
|
摘要点击次数: 2165 |
全文下载次数: 13 |
中文摘要: |
研究改性203树脂在半钢子午线轮胎胎侧胶中的应用。结果表明,在半钢子午线轮胎胎侧胶中使用改性203树脂等量替代R7510H树脂,胶料的焦烧时间略延长, t 90 略缩短,表面初始粘性和粘性保持率均有所提高,硫化胶60 ℃时的损耗因子明显减小,压缩疲劳温升和滚动阻力降低,其他物理性能相差不大。 |
英文摘要: |
The application of modified 203 resin in sidewall compound of steel-belted radial tire was studied.The results showed that,the modified 203 resin was used to equivalently replace the R7510H resin in the sidewall compound of steel-belted radial tire,the scorch time of the compound was slightly prolonged,the t 90 was slightly shortened,and the surface initial viscosity and viscosity retention rate of the vulcanizate increased,the loss factor at 60 ℃ was reduced,the temperature rise of compression fatigue decreased,and other physical properties were similar. |
|