文章摘要
Preparation and Performance Study of Flexible Electromagnetic Shielding Anti mold Coating Materials
Received:November 29, 2023  Revised:December 06, 2023
DOI:10.12136/j.issn.1000-890X.2025.02.0126
Key Words: electromagnetic shielding coating materials;antibacterial activity;adhesive performance;shielding performance
Author NameAffiliationE-mail
Li Bingzhang* The Thirty-third China Electronics Technology Group Corporation lbz0131@126.com 
Su Jiafeng 山西医科大学口腔医院  
Fan Jinfeng The Thirty-third China Electronics Technology Group Corporation  
Li Jing The Thirty-third China Electronics Technology Group Corporation  
Zhang Guien The Thirty-third China Electronics Technology Group Corporation  
Zhang Xiaogang The Thirty-third China Electronics Technology Group Corporation  
Hits: 238
Download times: 129
Abstract:
      A flexible electromagnetic shielding anti mold coating material(electromagnetic shielding coating material)was prepared and its properties were studied.The results showed that the electromagnetic shielding coating material prepared with a viscosity of 15 000 MP·s of methyl vinyl liquid silicone rubber,a dosage of 5 ‰ of 2-bromo-2-nitro-1,3-propanediol,1% of mold inhibitor,69.35% of conductive powder,and 7.38% of mineral oil had the best comprehensive performance.Its electromagnetic shielding efficiency was≥60 dB(10 MHz~10 GHz),shear strength was 0.95 MPa,peel force was 13.46 N·cm-1,and antibacterial performance reached level Ⅰ.It could effectively meet the requirements of low viscosity,good adhesion,excellent shielding performance,and good antibacterial performance of electromagnetic shielding coating materials when used in extreme environments.