Study on Tear Strength of EPDM and NBR at High Temperature
Received:April 10, 2018  Revised:April 10, 2018
DOI:10.12136/j.issn.1000-890X.2019.06.0413
Key Words: tear strength;high temperature;RT/HT tear strength ratio;EPDM;NBR;NR
Author NameAffiliationE-mail
ZHAO Xianghui* Xiamen Elastec Corp bradzhou@163.com 
YU Bo Xiamen Elastec Corp  
XIE Jintao Xiamen Elastec Corp  
ZHENG Tianlai Xiamen Elastec Corp  
Hits: 1109
Download times: 465
Abstract:
      The tear strength of ethylene-propylene-diene rubber(EPDM) and nitrile butadiene rubber(NBR) at different temperatures was studied. The results showed that the tear strength of EPDM and NBR compound decreased as temperature increasing,which basically conformed to Arrhenius equation. The tear strength at room temperature(RT) was about four times of that at high temperature(HT).Through the ratio of the tear strength at room temperature to high temperature(RT/HT tear strength ratio),the tear strength at high temperature could be directly calculated from the tear strength at room temperature.NR had higher tear strength at high temperature,so the tear resistance of other kinds of rubber at high temperature could be improved by blending NR.
View Full Text   View/Add Comment  Download reader
Close