Effect of pyrolysis temperature on surface area of carbon blacks recovered from natural rubber vulcanizate |
Received:October 31, 2016 Revised:October 31, 2016 |
DOI: |
Key Words: natural rubber vulcanizate, recovered carbon blacks;pyrolysis temperature;surface area;carbon black identification |
Author Name | Affiliation | E-mail | Qi Sheng-kai* | Stone Testing Technology | qi_shengkai@126.com | Zhang Yan-ling | 思通检测技术有限公司 | | Cao Cui-ling | 思通检测技术有限公司 | | Wu Ai-qin | 思通检测技术有限公司 | |
|
Hits: 957 |
Download times: 410 |
Abstract: |
Surface area of carbon blacks which were recovered from cured natural rubber at different pyrolysis temperatures has been measured,the results show that surface area increases with increasing pyrolysis temperature. Test surface area of the other pyrolytic carbon blacks at the pyrolysis temperature of 550℃, the results could be served as reference and guidance for unknown carbon black identification. |