文章摘要
Preparation of Regenerated Rubber Based Thermoplastic Elastomer
Received:July 16, 2015  Revised:July 16, 2015
DOI:
Key Words: regenerated rubber;thermoplastic elastomer;physical property
Author NameAffiliationE-mail
DUAN Youshun Key Lab of Rubber-plastics,Ministry of Education/Shandong Provincial Key Laboratory of Gum-plastics,Qingdao University of Science and Technology 36138634@qq.com 
WANG Yan Key Lab of Rubber-plastics,Ministry of Education/Shandong Provincial Key Laboratory of Gum-plastics,Qingdao University of Science and Technology  
YU Yang Key Lab of Rubber-plastics,Ministry of Education/Shandong Provincial Key Laboratory of Gum-plastics,Qingdao University of Science and Technology  
XIA Lin* Key Lab of Rubber-plastics,Ministry of Education/Shandong Provincial Key Laboratory of Gum-plastics,Qingdao University of Science and Technology xialin@qust.edu.cn 
XIN Zhenxiang Key Lab of Rubber-plastics,Ministry of Education/Shandong Provincial Key Laboratory of Gum-plastics,Qingdao University of Science and Technology  
Hits: 1392
Download times: 764
Abstract:
      The regenerated rubber based thermoplastic elastomer was prepared.The results showed that,using polystyrene-Polyethylene polybutene polystyrene(SEBS) as the continuous phase,and regenerated rubber as the dispersed phase,the comprehensive physical properties of regenerated rubber based SEBS thermoplastic elastomer were better,when the formula was SEBS 70,regenerated rubber 30,carbon black N330 10,Zinc Oxide 3,stearic acid 1,xylene 0.5,antioxidant 4010NA 1.5,accelerator TMTD 0.5,sulfur 0.5.