| 洪宗跃,阙元元.425/65R22.5 20PR 165K中长途卡客车轮胎的设计[J].轮胎工业,2026,46(8):0458-0461 |
 二维码(扫一下试试看!) |
| 425/65R22.5 20PR 165K中长途卡客车轮胎的设计 |
| Design of Medium and Long-Distance 425/65R22.5 20PR 165K Truck and Bus Tire |
| 投稿时间:2025-01-03 修订日期:2025-02-08 |
| DOI: |
| 中文关键词: 卡客车轮胎 结构设计 施工设计 成品轮胎性能 |
| 英文关键词: truck and bus tire structure design construction design finished tire performance |
| 基金项目: |
| 中图分类号: |
|
| 摘要点击次数: 78 |
| 全文下载次数: 27 |
| 中文摘要: |
| 介绍425/65R22.5 20PR 165K中长途卡客车轮胎的设计。结构设计:外直径 1 122 mm,断面宽 420 mm,行驶面宽度 332 mm,行驶面弧度高 10 mm,胎圈着合直径 569.5 mm,胎圈着合宽度 336 mm,断面水平轴位
置(介绍425/65R22.5 20PR 165K中长途卡客车轮胎的设计。结构设计:外直径 1 122 mm,断面宽 420 mm,行驶面宽度 332 mm,行驶面弧度高 10 mm,胎圈着合直径 569.5 mm,胎圈着合宽度 336 mm,断面水平轴位
置(H1/H2) 0.96,胎面采用5条连续的沟槽花纹,花纹深度 18 mm,花纹饱和度 74.97%,花纹周节数 46。施工设计:胎面采用全分层设计,1#—3#带束层使用3×0.2+6×0.35HT钢丝帘线,4带束层使用5×0.35HI钢丝帘线,胎体使用0.25+6+12×0.225HT钢丝帘线,钢丝圈采用斜六角形结构,采用一次法三鼓成型机成型、平板硫化机工艺硫化。成品轮胎的性能试验结果表明,轮胎的充气外缘尺寸、强度性能和耐久性能均符合设计和国家标准要求。
) 0.96,胎面采用5条连续的沟槽花纹,花纹深度 18 mm,花纹饱和度 74.97%,花纹周节数 46。施工设计:胎面采用全分层设计,1#—3#带束层使用3×0.2+6×0.35HT钢丝帘线,4#带束层使用5×0.35HI钢丝帘线,胎体使用0.25+6+12×0.225HT钢丝帘线,钢丝圈采用斜六角形结构,采用一次法三鼓成型机成型、平板硫化机工艺硫化。成品轮胎的性能试验结果表明,轮胎的充气外缘尺寸、强度性能和耐久性能均符合设计和国家标准要求。 |
| 英文摘要: |
| The design of medium and long-distance 425/65R22.5 20PR 165K truck and bus tire was described.In the structure design,the following parameters were taken:overall diameter 1 122 mm,cross-sectional width?420 mm,width of running surface 332 mm,arc height of running surface 10 mm,bead diameter at rim seat?569.58 mm,bead width at rim seat?336 mm,maximum width position of cross–section( H/1/H/2)?0.96,adopting 5 continuous grooves pattern for tread,pattern depth?18 mm,block/total ratio?74.97%,and number of pattern pitches?46.In the construction design,the following processes were taken:using a fully layered design for tread,using 3×0.2+6×0.35HT steel cord for 1#—3# belt,using 5×0.35HI steel cord for 4# belt,using 0.25+6+12×0.225HT steel cord for carcass,using oblique hexagonal structure for bead,using a one-stage three-drum building machine to build tires and a flat vulcanizing press to cure tires.The results of the finished tire performance test showed that,the inflated peripheral dimention,strength and durability met the requirements of corresponding design and national standards. |
|
|