文章摘要
梁英,姚秀红,李葆忠,苏忠铁.载重子午线轮胎外观明疤产生原因及解决措施[J].轮胎工业,2004,(6):344-346 本文二维码信息
二维码(扫一下试试看!)
载重子午线轮胎外观明疤产生原因及解决措施
Causes for appearance defects of BTR tire and their countermeasures
  
DOI:
中文关键词: 全钢载重子午线轮胎  外观明疤
英文关键词: BTR tire  appearance defect
基金项目:
中图分类号:U463.341+.3;U463.341+.6
作者单位
梁英 桦林轮胎股份有限公司 
姚秀红 桦林轮胎股份有限公司 
李葆忠 桦林轮胎股份有限公司 
苏忠铁 桦林轮胎股份有限公司 
摘要点击次数: 750
全文下载次数: 535
中文摘要:
      分析全钢载重子午线轮胎胎冠、胎侧、胎肩和胎圈部位外观明疤的产生原因,并提出解决措施。通过采取严格控制半成品部件尺寸、成型位置和硫化定型压力,正确使用隔离剂和内喷涂剂,定期清洗模具,杜绝内压水泄漏和外压蒸汽回窜等措施,取得了良好效果。
英文摘要:
      The causes for the appearance defects on crown,shoulder and bead areas of BTR tire were analyzed and their countermeasures were proposed.The appearance quality of BTR tire was significantly improved by taking the following measures:strictly control the dimensions and locations of tire components and the shaping pressure of green tire,properly apply the releasing agent and lubricant,regularly clean the mold,and protect the overheated water from leakage and the steam from reversing.
Author NameAffiliation
LIANG Ying Hualin Tire Co., Ltd 
YAO Xiuhong Hualin Tire Co., Ltd 
LI Baozhong Hualin Tire Co., Ltd 
SU Zhongtie Hualin Tire Co., Ltd 