对7.50-16 14PR轻型载重轮胎的胎冠和胎体胶配方进行优化设计,以进一步提高轮胎的耐久和耐磨性能。胎冠胶采用SBR代替充油丁苯橡胶,提高耐磨性能;胎体胶取消BR,内层与外层帘布胶统一为一个配方,保持良好的胎体性能,降低成本。 |
英文摘要: |
The formulation of crown compound and carcass ply compound for 7.50-16 14PR tire was optimized to improve the endurance and wear resistance.The NR/BR/OESBR blend was replaced by the NR/BR/SBR blend in crown compound to improve the wear resistance;and the NR/SBR/BR blend was replaced by the NR/SBR blend in carcass ply compound,and the same formula was used in both inner ply and outer ply compounds to obtain good performance of carcass and reduce the cost. |
|