12.00-20 16PR超加厚光胎面(L-5S)工程机械轮胎设计改进 |
Design modification of 12.00-20 16PR OTR tire withsuper thick smooth tread |
|
DOI: |
中文关键词: 〗工程机械轮胎 施工设计 成型机头 帘线假定伸张值 胎冠帘线角度 |
英文关键词: OTR tire construction design building drum presumed cord tension cord angle at crown |
基金项目: |
中图分类号:U463.341+.5 |
|
摘要点击次数: 971 |
全文下载次数: 18 |
中文摘要: |
分析12.00-20 16PR超加厚光胎面(L-5S)工程机械轮胎存在的成型卸胎坯困难、硫化后成品一次检验外观合格率低及充气外直径偏小等问题的产生原因,通过采取改用Φ690 mm全折叠式成型机头、增大胎面下层宽度、减小帘线假定伸张值和胎冠帘线角度及增加排气线与排气孔等措施,轮胎成品外缘尺寸达到设计要求,外观一次合格率由不足60%提高至90%以上,且生产效率提高。 |
英文摘要: |
The causes for difficult removing of green tire after building,lower acceptance rate in appearance inspection of finished tire after vulcanization and smaller overall diameter of inflated tire were analysed.The overall diameter of finished tire met the design standard,the acceptance rate in appearance inspection increased from 60% to 90%,and the productivity also increased by taking the following measures:use Φ690 mm whole collapsible drum,increase the width of base tread,decrease the presumed cord tension and the cord angle at crown,and increase the number of escape hole and escapeline. |
|