联轴器楔形橡胶块的硫化工艺研究 |
Study on Vulcanization Process of Wedge-shaped Rubber Block for Coupling |
Received:January 30, 2024 Revised:January 30, 2024 |
DOI:10.12137/j.issn.2095-5448.2025.03.0146 |
中文关键词: 楔形橡胶块;骨架表面处理;硫化工艺;仿真分析 |
英文关键词: wedge-shaped rubber block;skeleton surface treatment;vulcanization process;simulation analysis |
基金项目: |
中图分类号: |
Author Name | Affiliation | E-mail | LU Xiangzhou* | Zhuzhou Times New Material Technology Co., Ltd | luxiangzhou_qust@163.com | HOU Ming | Zhuzhou Times New Material Technology Co., Ltd | | XIE Yanfei | Zhuzhou Times New Material Technology Co., Ltd | | DENG Jiao | Zhuzhou Times New Material Technology Co., Ltd | | WANG Yiliang | Zhuzhou Times New Material Technology Co., Ltd | | ZHANG Yongchao | Zhuzhou Times New Material Technology Co., Ltd | | FANG Liang | Zhuzhou Times New Material Technology Co., Ltd | | WEN Taidou | Zhuzhou Times New Material Technology Co., Ltd | | DONG Yadong | Zhuzhou Times New Material Technology Co., Ltd | |
|
Hits: 225 |
Download times: 100 |
中文摘要: |
研究轨道车辆D360联轴器楔形橡胶块的硫化工艺。对楔形橡胶块骨架喷砂、除尘、涂胶等工序进行了针对性的优化,金属与橡胶粘接良好;采用Sigmasoft软件对楔形橡胶块的硫化时间和硫化温度进行精细化仿真,得出在143 ℃下硫化30 min时,楔形橡胶块性能稳定,外观及性能满足设计及使用要求。 |
英文摘要: |
The vulcanization process of wedge-shaped rubber block for D360 coupling of rail vehicle were studied.The targeted optimization were carried out on the sandblasting,dust removal,and glue coating processes of the wedge-shaped rubber block skeleton,and the bonding property between metal and rubber was good.The fine simulation of the vulcanization time and vulcanization temperature of wedge-shaped rubber blocks was carried out using Sigmasoft software,and it was found that after vulcanized for 30 minutes at 143 ℃,the appearance and performance of the wedge-shaped rubber block were stable and met the design and usage requirements. |