同向啮合双螺杆挤出机制备高性能环保再生橡胶及其性能研究
Preparation and Property of High Performance and Environmentally Friendly Recycled Rubber by Co-rotating Twin Screw Extruder
Received:May 08, 2020  Revised:May 15, 2020
DOI:10.12137/j.issn.2095-5448.2020.09.0516
中文关键词: 废旧轮胎;胶粉;再生橡胶;双螺杆挤出机;物理性能;古马隆树脂;固体无味油
英文关键词: waste tire;rubber powder;recycled rubber;twin screw extruder;physical property;coumarone resin;solid odorless oil
基金项目:
中图分类号:
Author NameAffiliationE-mail
QIANG Jinfeng* 1.Anhui GVG New Material Co.,LTD,Anhui Ma’anshan 243000
2.Anhui GVG Intelligent Equipment Co.,LTD,Anhui Ma’anshan 243000 
413526707@qq.com 
LI Guang 1.Anhui GVG New Material Co.,LTD,Anhui Ma’anshan 243000
2.Anhui GVG Intelligent Equipment Co.,LTD,Anhui Ma’anshan 243000 
 
FEI Dazhuang 1.Anhui GVG New Material Co.,LTD,Anhui Ma’anshan 243000
2.Anhui GVG Intelligent Equipment Co.,LTD,Anhui Ma’anshan 243000 
 
LI Tao 1.Anhui GVG New Material Co.,LTD,Anhui Ma’anshan 243000
2.Anhui GVG Intelligent Equipment Co.,LTD,Anhui Ma’anshan 243000 
 
RUI Guisheng 1.Anhui GVG New Material Co.,LTD,Anhui Ma’anshan 243000
2.Anhui GVG Intelligent Equipment Co.,LTD,Anhui Ma’anshan 243000 
 
JIANG Shuijin 1.Anhui GVG New Material Co.,LTD,Anhui Ma’anshan 243000
2.Anhui GVG Intelligent Equipment Co.,LTD,Anhui Ma’anshan 243000 
 
Hits: 1291
Download times: 0
中文摘要:
      用同向啮合双螺杆挤出机对废旧轮胎全胎胶粉进行剪切脱硫,制备高性能环保再生橡胶,考察挤出工艺、补强树脂和软化剂的种类与用量对再生橡胶性能的影响。结果表明:挤出最佳工艺参数为机筒第1—13区温度为140/140/70/190/130/120/110/110/100/110/100/90/80 ℃,螺杆转速为140 r·min-1;与添加植物系软化剂的再生橡胶相比,添加矿物系软化剂固体无味油的再生橡胶物理性能更好;添加4份古马隆树脂作为补强剂,10份固体无味油作为软化剂,制备的再生橡胶物理性能最好。
英文摘要:
      High performance and environmental friendly recycled rubber was prepared by shear desulfurization of waste tire powder by co-rotating twin screw extruder.The effects of extrusion process,type and amount of reinforcing resins and softeners on the properties of recycled rubber were investigated.The results showed that the optimum extrusion process parameters were as follows:the temperature in zone 1—13 was 140/140/70/190/130/120/110/110/100/100/90/80 ℃,and the screw speed was 140 r·min-1.The physical properties of the recycled rubber with mineral softener and solid odorless oil were better than those with plant softeners,the physical properties of the recycled rubber filled with 4 phrs of coumarone resin as reinforcing agent and 10 phrs of solid odorless oil as softener were the best.